Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4876
1
1
I work for a small company as an apprentice. We build ...
- Oct 20, 2021
by
korb23
Why not do the other side first.
And paste the pins from the...
- Oct 20, 2021
by
Stephen
as its a customer product we cant change much of the process...
- Oct 21, 2021
by
korb23
Could you provide us with more informations about this issue...
- Oct 21, 2021
by
Djo
Why is your customer controlling your process? You should b...
- Oct 21, 2021
by
jdengler
I'm not clear on your current process. You run FIRST SIDE. ...
- Oct 27, 2021
by
ProcEng1
Down-size or stagger the pin holes to "grab" the p...
- Oct 28, 2021
by
Tom
Or press fit.
But he said he can't change the pins or the bo...
- Oct 28, 2021
by
Stephen
Then adhesive or a pallet to support the header are the only...
- Oct 29, 2021
by
Tom