Using oxygen absorbers/scavengers to remove the need for nitrogen storage of sensitive parts

Views: 1116

#87297

Alternative to nitrogen atmosphere cabinet for storage of parts | 12 November, 2021

Hi SMTnet. I have a series of sensitive parts and solder preforms which degrade when exposed to oxygen and moisture. It seems the standard way of protecting these components is to use a nitrogen purged cabinet as storage.

This seems to use a lot of nitrogen as there is normally a constant flow of nitrogen through this enclosure. If it has an oxygen sensor inside to regulate the flow then it becomes a rather expensive piece of equipment. Does anyone know of the normal equipment that I would need to nitrogen purge and seal ESD bags with components within? Also, would using a dessicant and oxygen scavanger/absorber tablets be a suitable alternative? Thanks!

reply »

#87298

Alternative to nitrogen atmosphere cabinet for storage of parts | 12 November, 2021

Hi Jerry

We do sell hybrids cabinets nitrogen purge timer up to 20 minutes Or constant Capability of both To < 1% relative humidity and dessicating dryers in the same cabinet...

reply »

  • SMTnet
  • »
  • Electronics Forum
  • »
  • Using oxygen absorbers/scavengers to remove the need for nitrogen storage of sensitive parts
See Your 2024 IPC Certification Training Schedule for Eptac

Reflow Oven