Hello! Anyone here knows is there any specific time frame (... - Apr 14, 2022 by Evelyn
depends on board finish and PCB substrate materials. If you ... - Apr 14, 2022 by cbart
Thank you for sharing the helpful information. Let's say th... - Apr 15, 2022 by Evelyn
Bake a board. Measure weight. Measure board weight that have... - Apr 15, 2022 by Evtimov
So you run one side, and leave the boards sit in temperature... - Apr 18, 2022 by ProcEng1
Be aware that some "water soluble" fluxes can be c... - Apr 18, 2022 by charliem
Be careful of MSL level 4 or higher devices on the first sid... - Apr 19, 2022 by DWL
Alright. Thank you Evtimov :) ... - Apr 20, 2022 by Evelyn
@ProcEng1 Yea. Mostly is ENIG surface finished PCB. Sometime... - Apr 20, 2022 by Evelyn
@charliem, For the clean process board using "water... - Apr 20, 2022 by Evelyn
@DWL, Roger that. Thank you for your advice :) ... - Apr 20, 2022 by Evelyn