Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi
Sorry my poor english
We have some problems with some c...
- Dec 21, 2000
by
If you have a known problem with the parts, then Reject the...
- Dec 26, 2000
by
acahill
Your English is fine.
Your assessment that corrosion on a ...
- Dec 26, 2000
by
davef
Alejandro Rodriguez Gallegos