Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3828
We produce a two layer PCB which is on a .062" board ma... - Oct 13, 2022 by PRoy
Do you have the ability to add copper thieving or otherwise ... - Oct 13, 2022 by ProcEng1
No we can't change any of the copper, and that I believe is ... - Oct 13, 2022 by PRoy
I also believe it is the cause of the issue. I guess you co... - Oct 13, 2022 by ProcEng1
If you are running resonable volumes of the board, redesign ... - Oct 13, 2022 by sarason
What about warpage before reflow? Often the boards with unba... - Oct 19, 2022 by Andrey_F
If any changes in design is not possible and you have to sol... - Oct 19, 2022 by Andrey_F
Low Temp solder and a cooler profile should certainly help. ... - Oct 19, 2022 by ProcEng1
Thank you all a but the easy fix - of correcting copper - is... - Oct 19, 2022 by PRoy
I'm sorry to say, but it sounds like your bosses need a real... - Oct 19, 2022 by ProcEng1
I can understand the situation, when there is now possibilit... - Oct 19, 2022 by Andrey_F
Just because you can't add copper to the board, doesn't mean... - Oct 31, 2022 by Evtimov