Plated hole to copper spacing | 23 November, 2022

I am having problem with plated hole-copper spacing. I don't know if the gap between plated hole and copper can meet the capacity of PCB manufacturers. My board have 0.5oz copper weight on outer layer and distance of 0.177MM between plated hole and copper. Is there a standard table to check this distance by copper weight?