Hello,
We use OSP-finished PCB. One component (transformer) ...
- Dec 25, 2022
by
Rifat
Certainly, you need to take proper precautions in storing as...
- Dec 27, 2022
by
davef
How many assemblies you will have and how many transformers ...
- Jan 03, 2023
by
MagyarT
Hello,
It's around 10,000 assemblies & 1 transformer/ass...
- Jan 03, 2023
by
Rifat
As Davef mentioned above, I would be very precautious too wi...
- Jan 03, 2023
by
MagyarT
If you haven't opened the boards yet, don't.
OSP is the leas...
- Jan 03, 2023
by
Stephen
Hello Magyar, the main reason is supply chain disruption due...
- Jan 04, 2023
by
Rifat
Hello Magyar, the main reason is supply chain disruption due...
- Jan 04, 2023
by
Rifat
Hello Stephen, thanks for the advice. We are producing LED T...
- Jan 04, 2023
by
Rifat
Hello Rifat,
We have had good success with ImAg finish up to...
- Jan 05, 2023
by
SMTA-64419298
SMTA
I would wait. Scrap the bare boards you have and order fres...
- Jan 06, 2023
by
jdengler