Hi, Have been observed the post reflow inductor skew which ... - Jan 07, 2023 by Venkataramanaiah
How big is the board? What is the thickness? How populated i... - Jan 09, 2023 by MagyarT
Molten metal has a high surface tension. If the pads are une... - Jan 09, 2023 by Stephen
Magyart is on the right track. Lots of variables. Can you ... - Jan 09, 2023 by ProcEng1