Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 5516
Hello All, We have a small selective solder machine from RPS...
- Apr 19, 2023
by
James V
What Purity is the N2?
...
- Apr 20, 2023
by
ProcEng1
5 ppm from cylinders, thank you for taking the time to respo...
- Apr 20, 2023
by
James V
images? length of leads sticking out of pcb? pitch?
...
- Apr 21, 2023
by
bukas
I mean...there are a ton of possibilities for bridging on se...
- Apr 21, 2023
by
robgd3
I had also increased my flux to see if that helped, it did n...
- Apr 21, 2023
by
James V
Hi Rob, Yes I agree with everything stated. Lots of things c...
- Apr 21, 2023
by
James V
What kind of fume extraction are you using? If its too high,...
- Apr 21, 2023
by
DWL
It is pretty high, I will have to try it with no exhaust, th...
- Apr 21, 2023
by
James V
looks like low nitrogen to me
...
- Apr 24, 2023
by
bukas
Hi Bukas, thank you for taking the time to respond. My flow ...
- May 02, 2023
by
James V
I made a nitrogen nozzle from a starfrite silicone funnel an...
- May 02, 2023
by
James V
It was a nitrogen delivery issue. I used a funnel (silicone)...
- Jun 12, 2023
by
James V