I am looking for some tips of the trade with solder charges....
- Aug 07, 2023
by
QA123
To resolve this issue,
we use stencils with a step in the l...
- Aug 08, 2023
by
Dima
Did you struggle with bridging?
...
- Aug 08, 2023
by
QA123
What thickness did you go to and what aperture size did you ...
- Aug 08, 2023
by
QA123
We use 7mil step 35mil diameter.
Never got a bridges problem...
- Aug 09, 2023
by
Dima
thanks we will give it a try
...
- Aug 09, 2023
by
QA123
For which connectors? We are using a Andon BGA connector and...
- Aug 10, 2023
by
leeg
We are using a SAMTEC BGA connector.
...
- Aug 10, 2023
by
Dima