DDR5 SMD | 7 August, 2024

Has anyone encountered soldering DDR5 connectors in the SMD version? In the near future we are going to solder, they say that they warp when soldering, and in order to avoid defects they put a weight on them, hence the question, what to use as a load?

reply »

#91300

DDR5 SMD | 9 August, 2024

Placement jig which holds connector, SMD adhesive, profiling + low temperature paste. These are things I would research.

If these can be fitted in SMT, than these should also be JEDEC standard. Datasheets will offer you any information you need to be able to fit these and reflow them safely.

Regards, Tom

reply »