looking for cheap and useful solvent for ultrasonic stencil cleaner

jackie hsieh

#12093

looking for cheap and useful solvent for ultrasonic stencil cleaner | 1 April, 1999

dear all: we use the HCFC,manufactored by 3M,for the ultrasonic stencil cleaner.but it's too expensive to us. I think is it possible to use no-volatility liquid for the ultrasonic stencil cleaner? or other solvent?

thank for your help jackie hsieh

reply »

Jim Muckle

#12094

Re: looking for cheap and useful solvent for ultrasonic stencil cleaner | 5 April, 1999

Jackie:

We ran into some pretty ineresting guys at the Nepcon show who specialize in this area. It may be that they have a solution for you. Company name was Zestron, and the guy I spoke with was Andreas. Seemed very knowledgeable, and was very pleasant, not pushy. Number I have for him is 703-589-1198. Hope that helps.

| dear all: | we use the HCFC,manufactored by 3M,for the ultrasonic stencil cleaner.but it's too expensive to us. | I think is it possible to use no-volatility liquid for the ultrasonic stencil cleaner? | or other solvent? | | thank for your help | | jackie hsieh |

reply »

jackie hsieh

#12095

Re: looking for cheap and useful solvent for ultrasonic stencil cleaner | 5 April, 1999

dear jim, At first, thanks for your kindly help! Could you tell me the e-mail address of Andreas ? thanks again have a nice day!

| Jackie: | | We ran into some pretty ineresting guys at the Nepcon show who specialize in this area. It may be that they have a solution for you. Company name was Zestron, and the guy I spoke with was Andreas. Seemed very knowledgeable, and was very pleasant, not pushy. Number I have for him is 703-589-1198. Hope that helps. | | | | | | dear all: | | we use the HCFC,manufactored by 3M,for the ultrasonic stencil cleaner.but it's too expensive to us. | | I think is it possible to use no-volatility liquid for the ultrasonic stencil cleaner? | | or other solvent? | | | | thank for your help | | | | jackie hsieh | | |

reply »

Mike Konrad

#12096

Re: looking for cheap and useful solvent for ultrasonic stencil cleaner | 6 April, 1999

I would recommend the following chemistries:

Zestron Vigon SC200... Good but very $$$$ (703) 589-1198

Vertex (sold by Petrofirm and Alpha Metals)... Won't last as long as Zestron but must less $$$ (904) 261-8286

Kyzen... Also very good (800) 845-5524

I hope this helps.

If you have questions, feel free to call me toll-free at (800) 218-8128.

reply »

Bill Wilson

#12097

Re: looking for cheap and useful solvent for ultrasonic stencil cleaner | 6 April, 1999

JNJ Industries just came out with some real cool new chemistries for Ultrasonics at Nepcon called Aquasonic. You can contact them for info at 800-554-9994

| dear all: | we use the HCFC,manufactored by 3M,for the ultrasonic stencil cleaner.but it's too expensive to us. | I think is it possible to use no-volatility liquid for the ultrasonic stencil cleaner? | or other solvent? | | thank for your help | | jackie hsieh |

reply »

Circuit Board, PCB Assembly & electronics manufacturing service provider

Win Source Online Electronic parts