I looking for a possible rework on component terminals that... - Nov 08, 2000 by
First of all, verify your storage conditions. Its useful th... - Nov 08, 2000 by
ACI offers solderability restoration services by using Redu... - Nov 08, 2000 by CAL
You need to remove the oxide before you can properly solder... - Nov 08, 2000 by davef
Cristiano, Are your oxidised components now all on boards ... - Nov 09, 2000 by
Cristiano Dick Smiderle