Hi,
would like to get good info on the above solder pas...
- Aug 14, 2001
by
2% silver will be a little shinier. [Some inspectors hate t...
- Aug 14, 2001
by
davef
Basic understanding,
1) the 2% silver (Ag) gives better s...
- Aug 14, 2001
by
mugen
Say isn't creep a more key issue, rather than strength?
...
- Aug 14, 2001
by
davef
true....
tata why the elongation% is there.....
...
- Aug 14, 2001
by
mugen
But isn't elongation more of a quantification of ductility t...
- Aug 14, 2001
by
davef
Say din't someone previously claim,
"Dave F" stands for :
...
- Aug 16, 2001
by
mugen
Just feel relieved that we didn't go to the matt on the use ...
- Aug 16, 2001
by
davef
Pete