0201 solder beading

Steve B

#17663

0201 solder beading | 20 September, 2001

Have you seen any solder beading (balling) with the aperture sizes you have been using on 0201 components? Have you experimented with some of the solder bead reducing designs?

reply »

Jeff Schake

#17673

0201 solder beading | 21 September, 2001

I have observed solder balling for all aperture sizes tested. Solder balling levels appear to be better correlated against the amount of solder paste that is underneath the 0201 component terminations after placement rather than comparing this to the different aperture opening sizes. Generally, less material under the component will reduce solder balling. However, there has to be enough solder under the component to achieve a balanced and consistent wetting of the component terminations to solder reliably to the pads. Alternative aperture geometries, consisting of homeplate and bowtie shapes, were tested for transfer efficiency and print to print uniformity. These designs are intended to reduce the amount of solder printed under the component to inhibit the formation of satellite solder balls in reflow. The effectiveness of such a strategy to reduce solder balling for 0201s is still unclear to me, as the results so far are inconclusive. Using these alternative aperture shapes will typically reduce the volume capacity of the aperture, compared to a similar size rectangular opening. As a consequence, the aperture area ratio changes to a more challenging design, making it more difficult for the paste to release from the apertures. My argument for suggesting the use of rectangular apertures is based on this fundamental principle of maintaining tolerable area ratio levels. Compared to a rectangular aperture, the homeplate and bowtie shapes produced a much wider variation in print uniformity and lower transfer efficiency from the data collected. In turn, this was linked to lower assembly yields that may have masked any solder balling defects which otherwise would have occurred, making it difficult to determine if alternative aperture shapes did impact solder balling levels.

-Jeff

This message was posted Add this forum to your site! Click to learn more. the OnBoard Forums

reply »

Software for SMT

Fluid Dispensing Aerospace