Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
What is the best way/material to clean leads with 20% copper...
- Dec 05, 2001
by
smtspecialist
Now there�s a conundrum. You want the �best way to clean le...
- Dec 05, 2001
by
davef
Thanks for the info,
Of course the first thing to do was...
- Dec 06, 2001
by
No.
Assuming your talking the MG Chemicals product, MG Ch...
- Dec 06, 2001
by
davef
Yes it's a product from SG Chemicals, it does tin the leads ...
- Dec 07, 2001
by
Dull / shiny, I�m not sure that�s a proper indicator. If �L...
- Dec 07, 2001
by
davef
What is the composition of tin to lead in the "Liquid Tinner...
- Dec 11, 2001
by
Michael Parker
I have observed the same thing with solder composition in th...
- Dec 12, 2001
by