Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


Fine Pitch Rework

#18581

Fine Pitch Rework | 7 January, 2002

Hi!! I need some information about how to rework fine pitch components which had been rejected by machine and has coplanarity damage.

Does anyone know a procedure that can help me? Thanks in advance. Regards

reply »

#18590

Fine Pitch Rework | 7 January, 2002

Is your machine rejecting acceptable parts?

YES => Reprogram the machine NO => Search the fine SMTnet Archives, for instance: http://www.smtnet.com//forums/index.cfm?fuseaction=view_thread&CFApp=1&Thread_ID=2952&#Message12049&

reply »

mantis

#18606

Fine Pitch Rework | 8 January, 2002

Well assuming that the parts are genuinely damaged when rejected and you want to rework them to reduce scrap,you could use a shadow graph and get the mechanical spec on clear film.Then rework accordingly you should be able to rework most leads.

reply »


CAL

#18611

Fine Pitch Rework | 9 January, 2002

Remeber Do not use any probes or fixtures to hold the lead down while soldering or rework .....this is a bad idea. I would remove the component and replace or gently push the lead back into coplanarity and resolder. This all can be done at most rework stations. Dave posted a good question...Why is your PNP machine placing bad parts?

Cal Manncorp

reply »

JJFT

#18650

Fine Pitch Rework | 14 January, 2002

Also you have to be carefully because to many stress can damage the component internaly

reply »

Encapsulation Dispensing, Dam and Fill, Glob Top, CSOB