In the terminology of X-ray, does anyone know the meaning of...
- Feb 17, 2002
by
Daniel Woon
Dunno. Contact Gil Zweig ...
- Feb 19, 2002
by
davef
Do you mean middle height slice ? . This is a term used to d...
- Feb 19, 2002
by
Thanks Andy. BTW, is the HP5DX able to provide such measurem...
- Feb 21, 2002
by
Daniel Woon
Daniel,
The 5DX can indeed. You program the inspection h...
- Feb 21, 2002
by
JAX
The term is indeed "slice", Daniel. I am the 5DX engineer he...