Have QFP at o.5mm pitch with leads too oxidized for the flux...
- Mar 19, 2002
by
PeteC
We have had Corfin recommended to us, but have never needed ...
- Mar 19, 2002
by
davef
PETE -
Since you are local to ACI/EMPF you can take a run o...
- Mar 19, 2002
by
CAL
Thanks guys.
...
- Mar 20, 2002
by
PeteC
Our company carries out this service for major OEM and CEM's...
- Mar 28, 2002
by