Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi mates,
has anyone ever done a DoE on the degree of war...
- Jun 25, 2002
by
ianchan
We have not done a DOE on board warping. Consider:
* How c...
- Jun 26, 2002
by
davef
Hi Dave F,
customer calls it "warp", we can call it "twis...
- Jun 26, 2002
by
ianchan
Never did a DOE on that, but I think it would be quite diffi...
- Jun 27, 2002
by
Daan:
thanks for the tip.
...
- Jul 01, 2002
by
ianchan
What is Tg?
...
- Jul 01, 2002
by
Peterson
Tg = glass transition temperature, the temperature at which ...
- Jul 01, 2002
by
Remember! Empirical data will allow you to take advantage of...
- Jul 01, 2002
by
M Cox
ianchan