Suggestions are: * Convince yourself that your paste printing and paste control processes are in control. * Convince yourself you oven is in-control and capable. * Get one of those FREE software packages from the profiler companies [ie, KIC, ECD, etc]. We like the one from ECD. * Run the board with the canned recommendation from the FREE software packages from the profiler company. * Profile on the connections that don�t look good. * Read and follow the guidance of 7530 - Guidelines for Temperature Profiling for Mass Soldering (Reflow and Wave), nod three times in the general direction of Northbrook, IL, before taking a nap. * Leave work early because you�re doing such a good job. * Toss a coupla brats on the grill for me and blast Sousa on yer boom box �til the cops come.