Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi, Anybody with a solution on solder balls on gold pad. I h... - Jul 17, 2002 by computer
Search the fine SMTnet Archives to get started. ... - Jul 17, 2002 by davef
DaveF is correct in directing you to the archives. This prob... - Jul 17, 2002 by dragonslayr
Thks for the advise. ... - Jul 18, 2002 by computer
computer