Glue & Paste Printing on Same side of the PCB | 3 August, 2002

We are having 3 MPM UP-2000 printer & 1 AP-25 printer with us.

I would like to have the technical guidance for my following application.

For one of our model, there is a requirement of Glue & solder paste on same side of the PCB. Currently we are using glue dispenser & Solder paste printer for this. But glue dispensing takes lot of time & thruput becomes very less. So we want to go for Solder paste printing & glue printing on the same side of the PCB.

In this connection, my queries are :

1. What will be the process flow for this ?? 2. What kind of stencils, I have to use for Solder paste printing & glue printing ? 3. What kind of squeezee is to be used for Solder Paste & glue printing ? 4. Can our existing printers be used for this application ? 5. Any other guidlines.

This message was posted via the Electronics Forum @

reply »

#21049

Glue & Paste Printing on Same side of the PCB | 5 August, 2002

Just print solder paste first & then print adhesive with pump printing process (this is first invented by DEK).

RDGS

reply »

#21056

Glue & Paste Printing on Same side of the PCB | 6 August, 2002

OK, I'll bite.

How you can set a stencil down on a printed board and run a squeegee across it (even if it's a proflow head, it's still a squeegee, right?) without disturbing the printed paste?

reply »

#21058

Glue & Paste Printing on Same side of the PCB | 6 August, 2002

Hello Joseph,

How are you cleaning your Pump Print plastic stencils?

Regards, CN

reply »

matherat

#21064

Glue & Paste Printing on Same side of the PCB | 7 August, 2002

This sounds like it could be a SIPAD solid solder application.

Bring the boards in with the solderpaste already on them in a flattened solid form. Then you could print glue on them without disturbing wet paste.

1.Print glue. (Might take a little different stencil) 2.Place components in glue and onto the SIPAD ssd's 3.Spray flux? 4.Reflow

Might work, I'd have to see the design to be sure.

Matt Kehoe www.sipad.com

This message was posted via the Electronics Forum @

reply »

OhioD

#21082

Glue & Paste Printing on Same side of the PCB | 8 August, 2002

A "Pumpprint" stencil refers to a thick DEK stencil with pockets routed-out on the underside, so it will clear any THT leads, paste/glue deposits, etc., and not squish them. It's called pummprint because it was developed to use the ProFlow-type head (although you theoretically can use blades).

reply »

#21090

Glue & Paste Printing on Same side of the PCB | 9 August, 2002

Ahhh, OK, now I see. Seems like the pump would be a necessity, though, given that the aspect ration is going to go the wrong way.