Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
I have a question for everyone about component baking. In m...
- Aug 16, 2002
by
Ken Bliss
Baking is more like damage control than a preventative measu...
- Aug 16, 2002
by
davef
Hi Dave
Interesting points. If I understand you correctl...
- Aug 16, 2002
by
Ken Bliss
Clarifying:
1. About 2% of part numbers have a moisture pro...
- Aug 17, 2002
by
davef
What is the correct method to bake or cure the component?Sta...
- Aug 21, 2002
by
bayanbaru
I have never heard about a requirement for temperature ramp-...
- Sep 03, 2002
by
fmonette
...
- Sep 12, 2002
by
Stephen
"In theory there is no difference between theory and practic...
- Sep 12, 2002
by
Steve Thomas
I found the article online that I was talking about. It was...
- Sep 12, 2002
by
Stephen
Ken Bliss