Problem: Flux remains on the board in the masked areas aft... - Aug 21, 2000 by Ron H
Question: Do you run your pallets hot or cold thru the wave... - Aug 21, 2000 by James
The board and pallet are at room temperature when they pass... - Aug 21, 2000 by Ron H
Ron:It�s tricky to get what you want with this foamfluxers ... - Aug 22, 2000 by Wolfgang Busko
Actually Wolfgang that's what I was getting at. We use pal... - Aug 22, 2000 by James
Hi James, the problem is, it�s not gonna work with foam flu... - Aug 22, 2000 by Wolfgang Busko
James, I'm a little curious about your wave solder process.... - Aug 22, 2000 by Ron H
Me too. It was the first time that I heard about that "preh... - Aug 24, 2000 by Wolfgang Busko
Ok, here's why we preheat. In my limited experience at our... - Aug 24, 2000 by James
I see that it�s not a well intended process you run, just b... - Aug 24, 2000 by Wolfgang Busko