Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
greetings all Does anybody have any methods or recomendat... - Sep 27, 2002 by RDR
Russ, I have been reworking BGA's for over five years now an... - Sep 30, 2002 by Reworkman
Russ, first step would be to get IPC-7095 on BGAs. A f... - Sep 30, 2002 by Ioan Tempea
Hi, The acceptance level for voids is 25% and most of i... - Sep 30, 2002 by
thnaks everyone for the the input. I have been noticing tha... - Oct 07, 2002 by RDR
Russ, this post doesn't specificly address your original pos... - Oct 07, 2002 by David Razorsek
David, Guess what, Today I happened to try my new sample... - Oct 07, 2002 by RDR
Russ, I use the R562, it has a longer tack time then the Hm... - Oct 08, 2002 by LarryK
Hey Russell. The boys at Air-Vac Engineering can help you s... - Oct 08, 2002 by AJ
okay, so how does the DRS remove voids from BGAs? ... - Oct 09, 2002 by RDR
Russ, as I told Eric the other day ... The steadfast rule... - Oct 09, 2002 by davef
I guess you don't use one. Call them and I'm sure they will... - Oct 09, 2002 by AJ
AJ, I have bought and used 2 DRS24's in the past. It is a ... - Oct 09, 2002 by RDR
Dave, so for example I need to peak at 203 and hold for 5-10... - Oct 09, 2002 by RDR
Russ, Be careful on how you determine your liquidous poi... - Oct 09, 2002 by davef
"Do you work for Air-Vac or what?" My question as well. ... - Oct 10, 2002 by Steve Thomas
The whole thread seem's to have gone off track. Russ we've ... - Oct 19, 2002 by JohnW
Good points, John. Continuing to track on the voiding iss... - Oct 19, 2002 by davef
Dave, I've had a few intersting conversations with Dr Lee... - Oct 20, 2002 by JohnW