This one's got me stumped, so I thought I'd throw it out for... - Nov 05, 2002 by Ray Morford
This sounds like a contamination issue with the HASL finish.... - Nov 05, 2002 by RDR
This defect is there after reflow. My first thought was tha... - Nov 06, 2002 by Ray Morford
First, from what you say, it's unclear that there is a "sold... - Nov 06, 2002 by davef
Nothing funny seems to happen to the connector when heated. ... - Nov 06, 2002 by Ray Morford
I hear you on the profiling issue. That won't get at the is... - Nov 06, 2002 by davef