Hello!! I have a questions about what kind of squeegee blad... - Nov 24, 2002 by Beto Hdz
Hello!! I have a question about what kind of squeegee blade... - Nov 24, 2002 by Beto Hdz
Now that is a BIG step. Stencil type: * A metal squeegee... - Nov 25, 2002 by davef
In my haste to respond, I neglected to ask THE QUESTION. ... - Nov 27, 2002 by davef
I wouldn't recommend a metal squeegee, because if you can't ... - Dec 06, 2002 by Daan
Hi I can image too many images for what your product or y... - Dec 09, 2002 by
You want to use a rubber squeegee with as high as a duromete... - Dec 09, 2002 by swagner
Hello. Sometimes metal squeegees DO work with stepped stenc... - Jan 02, 2003 by