Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
We're trying a selective soldering pallet for the first time... - Dec 02, 2002 by Steve Thomas
Hi Steve The people who will have the answer is the exper... - Dec 02, 2002 by
If you can, attach athermocouple to the locations where you ... - Dec 02, 2002 by RDR
Unfortunately it's nc or we'd be worrying about this on the ... - Dec 02, 2002 by Steve Thomas
Steve, I agree with the recommendation to check the tempera... - Dec 02, 2002 by
Hi, Try to check if there is water absorbed in the flux ... - Dec 02, 2002 by Kris
We haven't run a profile yet....probably because we're a-f... - Dec 03, 2002 by Steve Thomas
This might be a trival mundane suggestion but try to use non... - Dec 03, 2002 by Kris
At the price of Durapol we'd never get the OK to have them m... - Dec 03, 2002 by Steve Thomas
I have found that preheating the solder pallets prior to use... - Dec 04, 2002 by James
By the way, what type of preheaters do you have? IR? Conve... - Dec 04, 2002 by
They're IR, bottom side only. Frankly wave solder is not my... - Dec 05, 2002 by Steve Thomas
Have you check the flux gravity lately? If not, Check the fl... - Dec 05, 2002 by
We only have solder balling problems in the interface of the... - Dec 06, 2002 by Steve Thomas
Steve, I wave solder most if not all our boards with sele... - Dec 10, 2002 by
Randy, Steve & all, Can you guys point me in the right di... - Dec 16, 2002 by
Jim Consider issuing a purchase order to your assembler f... - Dec 16, 2002 by davef
Steve , I agree with all the responses you have received. ... - Dec 16, 2002 by David Duke
Jim, In most cases if you can eliminate a process you wil... - Dec 17, 2002 by
There are a few emerging technologies that have been growing... - Dec 17, 2002 by robf