Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hello,
We recently installed a new/used UPK 650 fitted wi...
- Jan 23, 2003
by
hoss67
While not familiar with the flux, I'd increase the conveyor ...
- Jan 23, 2003
by
davef
How are these connectors and dips oriented? If the leads are...
- Jan 24, 2003
by
RDR
I sent you a couple of charts to assist with your troublesho...
- Jan 24, 2003
by
PeteC
I am not familiar with your flux but with no-cleans (which I...
- Jan 24, 2003
by
Hi,
Distance Engineering is always difficult.
I am gue...
- Jan 24, 2003
by
RMA needs to be dry prior to the wave to work. If coverage ...
- Jan 24, 2003
by
TriGuy
DDave,
I do not have the benefit of having the old machin...
- Jan 24, 2003
by
hoss67
Correction: The Ultrapak (UPK) 600 and Electra models allow ...
- Jan 24, 2003
by
PeteC
Hi
Again Distance is tough, besides far less exciting..
...
- Jan 24, 2003
by
I agree with most of the other suggestions here, but 90 C fo...
- Jan 28, 2003
by
MikeF
I've seen this problem on more than one wave,What i've done ...
- Jan 28, 2003
by
sajulius
Mike,
I've tried the high side of the flux preheat spec w...
- Jan 28, 2003
by
hoss67
Hi
Wow, I can't imagine this set up.
No wonder some of u...
- Jan 31, 2003
by
Dave,
I do have the mechanical drawings but no electronic...
- Jan 31, 2003
by
hoss67
I would go for the laminar flow as opposed to N2. The conto...
- Jan 31, 2003
by
RDR
Hoss, if you have trouble with finding the parts you need th...
- Jan 31, 2003
by
RDR
Russ,
Roger that.
Thanks.
...
- Jan 31, 2003
by
hoss67