I placed a micro bga using flux paste and ran it through my ...
- Feb 20, 2003
by
mdm4ua
Give us infortmation, please. What is [are]:
* Height boar...
- Feb 20, 2003
by
davef
Hi,
there is one very important thing.How many boards came ...
- Mar 21, 2003
by
Evtimov
Is it possible that the flux you used, if applied in excess ...
- Mar 21, 2003
by
RDR
Russ,
u mean excess flux causes "blow hole" defect?
...
- Mar 21, 2003
by
iman
I agree with Russ, seen this happen if the right amount of p...
- Mar 22, 2003
by
bcceng
I don't know if I would call it a "blow hole". what I belie...
- Mar 24, 2003
by
RDR