Hi all
Pls. help advise.
Our board use RMA solder paste...
- Mar 12, 2003
by
Por
Hi
I don't see in your note any particular reasons why yo...
- Mar 12, 2003
by
J-STD-001C, 7.2.1 Flux Application says words to the effect ...
- Mar 12, 2003
by
davef