Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Recent cross-section analysis for a customer complaint revea... - Apr 16, 2003 by
What was the original complaint? when you say solder wicked... - Apr 16, 2003 by RDR
Thanks Russ! The origianal complaint from the customer was ... - Apr 16, 2003 by
Thanks for the info, Here is a couple more questions (and yo... - Apr 16, 2003 by RDR
While Russ is correct that a little voiding is OK, your leve... - Apr 17, 2003 by davef
Russ, The caps are 0603 case size. I am not sure about the... - Apr 17, 2003 by
Thanks Dave! What level of voiding is acceptable? Would yo... - Apr 17, 2003 by
A-610 talks to acceptable voiding. ... - Apr 17, 2003 by davef
Takfire Questions are: * Why does your customer think th... - Apr 17, 2003 by davef
This is not quite what you're asking, but for BGA acceptance... - Apr 17, 2003 by davef
Background: * Bulwith, Ronald A., �Failure Analysis of Sold... - Apr 17, 2003 by davef
Dave, I am not exactly sure what is driving them to believe... - Apr 17, 2003 by
Dave, I truly appreciate your efforts in providing inform... - Apr 17, 2003 by
We undoubtedly will take you up on that offer. Please email... - Apr 17, 2003 by davef
Q1: Industry standard detailing solder joint quality? A1: A... - Apr 17, 2003 by davef
Takfire