Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Could anyone give me a basic profile temperature settings fo... - Jun 16, 2003 by
The second one is typical. The important temperature is the... - Jun 16, 2003 by Stephen
The main problem I am having is getting the Rising slope 1-3... - Jun 17, 2003 by
Hi The temprature for the first zone should be more as t... - Jun 24, 2003 by Sanjeev Chandra
The temprature for the first zone should be less as the PCB ... - Jun 24, 2003 by Stephen
So which one is it? I am getting confused a bit because the... - Jun 24, 2003 by
We have a 5 zone oven and were starting at 150 which brought... - Jun 25, 2003 by Stephen
This may make it easy, Do you really need soak? Or can you j... - Jun 25, 2003 by RDR
Water soluble pastes generally work best with a ramp-to-spi... - Jun 25, 2003 by
Hi James, I saw very good posts here.Now I will give you on... - Jun 26, 2003 by Evtimov
To Brian W. I think I will use your concept thanks for the ... - Jun 26, 2003 by
James