Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
We have an internal engineering study on blowhole solder joi...
- Jul 15, 2003
by
iman
I have done a DOE on the SMT components, not the BGA, for re...
- Jul 16, 2003
by
Blow holes/ pin holes in solder joints are the result of mul...
- Jul 21, 2003
by
Don,
thanks for the thoughtful insight, can I run some th...
- Jul 21, 2003
by
iman
Theory #6 [maybe 3a?]: If you change your paste to a 'non-vo...
- Jul 21, 2003
by
davef
Dave F,
thats' the path of thought we are now bumbling a...
- Jul 22, 2003
by
iman
Iman: Don't be too quick to judge. Most paste suppliers o...
- Jul 22, 2003
by
davef
Yo Thanks!
right on the money pad, the pinhole occurs mai...
- Jul 23, 2003
by
iman
There is much written on the effect of reflow recipe on void...
- Jul 23, 2003
by
davef
iman