Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Is jet dispensing of highly filled polymers possible? I hav... - Aug 05, 2003 by
Mike Stadt
#25361
jet dispensing highly-filled polymers | 5 August, 2003
Is jet dispensing of highly filled polymers possible? I have only seen applications with SMT adhesives, where the filler content is on the order of 10%.