Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi all,
We recently purchased an Omniflow 10 and I am set...
- Sep 04, 2003
by
Sr. Tech
Sr.
Assuming you are processing the garden variety 63/37 ...
- Sep 06, 2003
by
Thanks.
I have another question. I believe this machine w...
- Sep 08, 2003
by
Sr. Tech
Contact Electrovert on your questions- Tad Formella, ...
- Sep 08, 2003
by
The reason I am posting on this site is because Electrovert ...
- Sep 08, 2003
by
Sr. Tech
Oh, I see, concerning the fee. Sorry.
Running NitroCool wit...
- Sep 08, 2003
by
I had an Omni10 that was set up for nitrogen, but also requi...
- Sep 08, 2003
by
Yes I have cleaned the nitrogen knives out, and I have a chi...
- Sep 09, 2003
by
Sr. Tech
Se�or Tech: Exploring other options is good, but at the end ...
- Sep 09, 2003
by
davef
SR. Tech:
I have worked with Omniflo 7 and 10 ovens for m...
- Sep 18, 2003
by
donbell