Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Does anyone know of a good, cost effective protection for go...
- Dec 23, 2003
by
The fine SMTnet Archives are a GREAT resource. Two treads t...
- Dec 23, 2003
by
davef
Kapton tape is heat resistant to tempratures accociated with...
- Dec 24, 2003
by
Paul pmd
Paul: You are correct, but:
* No all Kapton tape suppliers...
- Dec 28, 2003
by
davef
We have do away with Kapton tape many years ago, now using t...
- Dec 29, 2003
by
If your proces is NC then you can use an Amonia-free laytex ...
- Dec 29, 2003
by
Yes,
We have done away with masking with kapton 8 yrs ago...
- Jan 02, 2004
by
gpaelmo
pquinney