I am a SMT biginner. can anybody tell me what is HASL board...
- Jun 29, 2000
by
Welcome Bob,
HASL stands for "Hot Air Solder Level" and is...
- Jun 29, 2000
by
Mark
Hi Bob, welcome
Let's take this a little further. You'll a...
- Jun 29, 2000
by
John Thorup
Thanks for your Input.
That helped me alot.
...
- Jun 29, 2000
by
BOB