Hi all,
We have a PCB without any BGAs on it which goes i...
- Feb 12, 2004
by
Why can't you conformally coat the BGA? We do on some of ou...
- Feb 12, 2004
by
we are worried about the coating not being able to cover und...
- Feb 13, 2004
by
You might want to check int using a BGA underfill material p...
- Feb 13, 2004
by
Underfills could improve reliability. If you pick materials...
- Feb 13, 2004
by
Kris