Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi,
I just need to undestand any issue? If I mount Pb free ...
- May 06, 2004
by
Vijay
Even with PbSn solderpaste the leadfree BGA's have a superio...
- May 06, 2004
by
davef
Any view on what the minimum reflow temperature is for a SAC...
- Jun 01, 2004
by
Lynn
profile it for the tin/lead paste.
The tin in the solder ...
- Jun 01, 2004
by
...oops part 2:
I will assume a sac 350 ball??? 217-218C...
- Jun 01, 2004
by
Is there not an issue with reflowign the SAC ball's in term'...
- Jun 02, 2004
by
johnwnz
Thanks to all on this feedback
...
- Jun 02, 2004
by
Lynn
Vijay