Alpha UP78 OSP problem

Melissa

#28534

Alpha UP78 OSP problem | 11 May, 2004

Has anyone experienced problems lately with excess flux residue left on the board after reflow when using Alpha UP78 OSP paste? We are getting a component failure that the designers are blaming on too much residue.

Thanks

reply »

#28535

Alpha UP78 OSP problem | 11 May, 2004

Nope, haven't heard anything. I'd check your reflow profile, contact Alpha. Also, UP78 is a very old solderpaste product. I would consider switching to one of their newer products.

reply »

#28540

Alpha UP78 OSP problem | 11 May, 2004

What is the problem with "too much residue"? How much residue is acceptable?

reply »

#28557

Alpha UP78 OSP problem | 12 May, 2004

When you say "very old" do you mean it's discontinued? My supplier is telling me they still sell it.

In this case, the residue is pooling up and clogging up a switch. That's what we are considering too much.

Thanks.

reply »

#28558

Alpha UP78 OSP problem | 12 May, 2004

Yes, old not obsolete. I believe it may be Alpha's first no-clean solderpaste model. Their most current NC model is OM 5000.

reply »