Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi I'm trying to plot a LSP profile to reduce void. But ... - Jun 06, 2004 by
Hi I'm trying to plot a LSP profile to reduce void. But ... - Jun 06, 2004 by
So what is LSP? ... - Jun 06, 2004 by RDR
Hi Russ I happen to come across a article about reflow pr... - Jun 07, 2004 by
LSP is 'Long Soak Profile'. See ... - Jun 07, 2004 by Mark Stansfield
ADM, just click on my name and it will give you the E-Mail. ... - Jun 07, 2004 by RDR
First, voiding is a process indicator. Next, as you say, th... - Jun 07, 2004 by davef
Me too. Check out this months Circuits Assembly. Dage has ... - Jun 07, 2004 by
Hi Russ I can't get your email address. I'm not a registe... - Jun 08, 2004 by
adm
adm