Hello,
I'd like to consult somebody here about how to do th...
- Aug 09, 2004
by
Do a search on COLD SOLDER and see if this answers some ques...
- Aug 09, 2004
by
Mark M.
The #1 cause of cold-solder is less heat.
...
- Aug 12, 2004
by
Solderability standards are:
* IPC EIA J-STD-002B - Soldera...
- Aug 13, 2004
by
davef
Sometimes cold solder can manifest if out of date solder pas...
- Aug 24, 2004
by
MM