leadfree connector

JJ

#30987

leadfree connector | 15 October, 2004

Hi, there

Any idea if leadfree through hole connector can be used in standard leaded process? If not, why ?

Thanks

reply »

T.E.A.M. Services

#30988

leadfree connector | 15 October, 2004

No lead devices oxidize very quickly when washed. Try to keep it a no clean process. Solderability comes into play a bit depending on solder paste.

reply »

#30992

leadfree connector | 16 October, 2004

Here is a thread from the fine SMTnet Archives from a couple of weeks ago, where we spoke about the topic of mixed lead-free solder with components that have lead-bearing solderability protection: http://www.smtnet.com/forums/Index.cfm?CFApp=1&Message_ID=30307