Can BGA's really be reliably attached without adding any ext... - Oct 31, 2004 by Matt Kehoe
I believe on High Temp. Spheres you require paste eutectic 6... - Oct 31, 2004 by
Yes, you can place a BGA in flux and get good reflow. Howev... - Nov 01, 2004 by
There is no IPC requirement for reworking BGA with either pa... - Nov 01, 2004 by davef
Good stuff! Thanks to all. mk ... - Nov 01, 2004 by Matt Kehoe
Agreed. You will find different part manufacturers have dif... - Nov 01, 2004 by
Isn't that a good reason to use more paste? With just the pa... - Nov 02, 2004 by Matt Kehoe
I have never experienced voids when using the flux only for ... - Nov 02, 2004 by RDR