Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi,
We would like to know on the IPC-A-610 rev. C standar...
- Nov 03, 2004
by
Dennis
Hi Dennis,
It is all dependant on what you state for the ...
- Nov 03, 2004
by
Hi Simon,
Thanks for the immediate reply. We really appre...
- Nov 03, 2004
by
Dennis
Hi Dennis,
I would say that you must meet one of the acce...
- Nov 03, 2004
by
Could you give a specific example (sect. paragraph etc) that...
- Nov 03, 2004
by
RDR
Hi Russ,
Thanks for the reply. In IPC-A-610 Rev. C on sec...
- Nov 03, 2004
by
Dennis
Dennis: The IPC-A-610 requirements are seperate.
* You n...
- Nov 03, 2004
by
davef
Hi Dave,
Thanks a lot for the clarification. In order to ...
- Nov 03, 2004
by
Dennis
As stated by others you are out of IPC compliance, However,...
- Nov 04, 2004
by
RDR
Hi Russ,
Thanks for the input. We already check our subco...
- Nov 04, 2004
by
Dennis