I am testing some BGA's (PBGA 30mm x 30mm) to evaluate the m...
- Dec 27, 2004
by
Hi,
Why are you worried about ramp rate on the BGA? Do yo...
- Dec 27, 2004
by
The ramp rate of the temperature of your solder is more impo...
- Dec 28, 2004
by
davef
No delta T issues as I am not actually reflowing the compone...
- Dec 28, 2004
by
Doesn't make sense. Either your:
* Oven is not operting pr...
- Dec 28, 2004
by
davef
Mark