Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Help!! Just got some new wave solder pallets in house. The ...
- Jan 12, 2005
by
Hi,
Are you coating the bottom of the palette with flux? ...
- Jan 12, 2005
by
Try scoring the underside of the pallet every inch or so, pe...
- Jan 12, 2005
by
Are you positive that the solder is sticking to the bottom o...
- Jan 12, 2005
by
RDR
Thanks for the replies. I use a foam fluxor, so the pallet ...
- Jan 12, 2005
by
I have seen the solder shoot out at least 4"-6" from both th...
- Jan 12, 2005
by
RDR
Sue,
What is the material your pallet is made of?? Are you...
- Jan 12, 2005
by
Chad Haima
How thick is this pallet?
6mm, 8mm, 10mm?
I would look a...
- Jan 12, 2005
by
The pallets are made of a black composite that is 5MM thick,...
- Jan 13, 2005
by
SuePH