Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Is there a procedure for the this test? If yes please forwar... - Jan 26, 2005 by Richard
Look here for more on dye & pry: ... - Jan 26, 2005 by davef
Richard
#32255
Die and Ply Procedure | 26 January, 2005
Is there a procedure for the this test? If yes please forward to me. Thx.
reply »
davef
#32271
Look here for more on dye & pry: http://www.smtnet.com/forums/Index.cfm?CFApp=1&Message_ID=25007